on front Aluminum/silicon/copper DC-magnetron sputtering (low power) |
|
Process characteristics: |
Thickness Amount of material added to a wafer |
|
Ambient Ambient to which substrate is exposed during processing |
vacuum |
Batch size |
1 |
Deposition rate Rate at which material is added to a wafer |
0.024 µm/min |
Excluded materials |
gold (category), copper |
Material |
aluminum/silicon/copper [98:1:1] |
Pressure Pressure of process chamber during processing |
5 mTorr |
Sides processed |
either |
Temperature |
27 °C |
Wafer size |
|
Equipment |
Denton Discovery 24 |
Equipment characteristics: |
Wafer holder Device that holds the wafers during processing. |
stainless steel |
Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
alumina, Borofloat (Schott), silicon, silicon dioxide |
Wafer thickness List or range of wafer thicknesses the tool can accept |
300 .. 1000 µm |
Comments: |
|
Extra terms |
Customer agrees that wafers, masks, and other materials
incorporating any process(es) provided by this fabrication site
are to be used solely for non-commercial research
purposes.
|